![szilícium-karbid golyóálló kerámia](https://siliconcarbide.net/wp-content/uploads/2017/12/silicon-carbide-bulletproof-ceramic-186x186.jpg)
this kind of silicon carbide bricks is made of super fine sintered silicon carbide powder with excellent thermal conductivity, high temperature resistant, high temperature resistant to oxidation, corrosion resistance, acid and alkali, solvent and other advantages, this kind of silicon carbide tiles as one kind best bulletproof vest is high strength, high wear resistance, can meet the military with ballistic panels, anti shock, a good agreement with the military bulletproof shield requirements of the lighter, stronger and more flexible policy.This kind sic tiles is a high-end protective armour. Sintered silicon carbide tiles has much stronger wear and strength resistance than reaction bonded silicon carbide bricks.we can make sic tiles according to your requirement.
Item Unit SSiC
Hardness HRA 94
Hardness HV 2500
Porosity Rate % <0.2
Density g/cm3 3.1-3.15
Compressive Strength Mpa >3000
Bending Strength Mpa >400
Coefficient of Expansion 10-6/℃ 4.3
Content of SiC % ≥99
Free Si % <0.1
Elastic Modulus Gpa 410
Temperature ℃ 1600