![keramické trysky na pieskovanie z karbidu kremíka](https://siliconcarbide.net/wp-content/uploads/2013/10/silicon-carbide-ceramic-sandblasting-nozzles-e1451740344597-186x186.jpg)
Reaction Bonded silicon carbide sandblasting nozzles
This SIC ceramic product has high hardness, high wear resistant
Main uses: the product can be used as sandblasting nozzle, water and sand cutting nozzle and the steel mill, power plant and other industries using coal nozzle. Its service life is 5-10 times of the ordinary material.