{"id":676,"date":"2026-04-03T15:47:58","date_gmt":"2026-04-03T07:47:58","guid":{"rendered":"https:\/\/siliconcarbide.net\/?p=676"},"modified":"2026-04-03T15:47:58","modified_gmt":"2026-04-03T07:47:58","slug":"%e7%82%ad%e5%8c%96%e3%82%b1%e3%82%a4%e7%b4%a0%e3%83%8e%e3%82%ba%e3%83%ab%e3%81%8c3d%e5%8d%b0%e5%88%b7%e3%81%ab%e9%81%a9%e3%81%97%e3%81%a6%e3%81%84%e3%82%8b%e7%90%86%e7%94%b1","status":"publish","type":"post","link":"https:\/\/siliconcarbide.net\/ja\/why-silicon-carbide-nozzle-work-better-in-3d-printing\/","title":{"rendered":"\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u304c3D\u30d7\u30ea\u30f3\u30c6\u30a3\u30f3\u30b0\u306b\u9069\u3057\u3066\u3044\u308b\u7406\u7531"},"content":{"rendered":"<h1>\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u304c3D\u30d7\u30ea\u30f3\u30c6\u30a3\u30f3\u30b0\u306b\u9069\u3057\u3066\u3044\u308b\u7406\u7531<\/h1>\n<p>\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306f\u3001\u4ed6\u306e\u30ce\u30ba\u30eb\u306b\u306f\u306a\u3044\u6027\u80fd\u3068\u8010\u4e45\u6027\u3092\u63d0\u4f9b\u3059\u308b\u3053\u3068\u3067\u30013D\u30d7\u30ea\u30f3\u30c8\u306e\u30b2\u30fc\u30e0\u3092\u5909\u3048\u307e\u3057\u305f\u3002\u3053\u308c\u3089\u306e\u30ce\u30ba\u30eb\u306f\u3001\u975e\u5e38\u306b\u786c\u304f\u3001\u9ad8\u6e29\u3067\u3082\u5b89\u5b9a\u3057\u3066\u3044\u308b\u3053\u3068\u3067\u77e5\u3089\u308c\u3066\u3044\u308b\u6750\u6599\u304b\u3089\u4f5c\u3089\u308c\u3066\u304a\u308a\u3001\u591a\u304f\u306e\u5370\u5237\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002\u3053\u306e\u8a18\u4e8b\u3067\u306f\u3001\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306e\u7279\u5225\u306a\u7279\u5fb4\u3001\u5f93\u6765\u306e\u6750\u6599\u3088\u308a\u3082\u512a\u308c\u3066\u3044\u308b\u70b9\u3001\u3055\u307e\u3056\u307e\u306a\u7523\u696d\u3067\u4f7f\u7528\u3067\u304d\u308b\u70b9\u3092\u898b\u3066\u3044\u304f\u3002.<\/p>\n<h2>\u70ad\u5316\u30b1\u30a4\u7d20\u3092\u77e5\u308b<\/h2>\n<p>\u70ad\u5316\u30b1\u30a4\u7d20\uff08SiC\uff09\u306f\u30b1\u30a4\u7d20\u3068\u70ad\u7d20\u306e\u7d44\u307f\u5408\u308f\u305b\u3067\u3001\u975e\u5e38\u306b\u8208\u5473\u6df1\u3044\u7269\u7406\u7684\u30fb\u5316\u5b66\u7684\u7279\u6027\u3092\u6301\u3064\u3002\u975e\u5e38\u306b\u786c\u304f\u3001\u71b1\u4f1d\u5c0e\u7387\u304c\u9ad8\u304f\u3001\u6469\u8017\u3084\u8150\u98df\u306b\u5f37\u3044\u3053\u3068\u3067\u77e5\u3089\u308c\u3066\u3044\u308b\u3002\u70ad\u5316\u30b1\u30a4\u7d20\u306f\u6700\u3082\u786c\u3044\u7d20\u6750\u306e\u3072\u3068\u3064\u3067\u3001\u30e2\u30fc\u30b9\u786c\u5ea6\u306f9.5\u3067\u3059\u3002\u3053\u308c\u3088\u308a\u786c\u3044\u7d20\u6750\u306f\u30c0\u30a4\u30e4\u30e2\u30f3\u30c9\u3060\u3051\u3067\u3059\u3002\u305d\u306e\u305f\u3081\u3001\u9577\u6301\u3061\u3057\u3001\u5f37\u5ea6\u304c\u5fc5\u8981\u306a\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002.<\/p>\n<h2>\u70ad\u5316\u30b1\u30a4\u7d20\u306e\u6700\u3082\u91cd\u8981\u306a\u7279\u5fb4<\/h2>\n<p>\u9ad8\u3044\u786c\u5ea6\uff1a\u70ad\u5316\u30b1\u30a4\u7d20\u306f\u975e\u5e38\u306b\u786c\u3044\u305f\u3081\u3001\u591a\u304f\u306e\u78e8\u8017\u3084\u640d\u50b7\u306b\u5bfe\u5fdc\u3067\u304d\u3001\u9ad8\u6027\u80fd\u306a\u7528\u9014\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002.<br \/>\n\u71b1\u5b89\u5b9a\u6027\uff1a\u70ad\u5316\u30b1\u30a4\u7d20\u306f1600\u2103\u307e\u3067\u306e\u6e29\u5ea6\u306b\u5bfe\u5fdc\u3067\u304d\u3001\u975e\u5e38\u306b\u9ad8\u6e29\u307e\u305f\u306f\u4f4e\u6e29\u306e\u6761\u4ef6\u4e0b\u3067\u3082\u5f37\u5ea6\u3092\u7dad\u6301\u3057\u307e\u3059\u3002.<br \/>\n\u8010\u98df\u6027\uff1a\u3053\u306e\u7d20\u6750\u306f\u5316\u5b66\u8150\u98df\u306b\u975e\u5e38\u306b\u5f37\u3044\u305f\u3081\u3001\u904e\u9177\u306a\u5834\u6240\u3067\u306e\u4f7f\u7528\u306b\u6700\u9069\u3067\u3059\u3002.<br \/>\n\u4f4e\u71b1\u81a8\u5f35\uff1a\u70ad\u5316\u30b1\u30a4\u7d20\u306f\u71b1\u81a8\u5f35\u7387\u304c\u4f4e\u304f\u3001\u6e29\u5ea6\u304c\u5909\u5316\u3057\u3066\u3082\u30b5\u30a4\u30ba\u304c\u3042\u307e\u308a\u5909\u308f\u308a\u307e\u305b\u3093\u3002.<\/p>\n<h2>\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306e\u5229\u70b9<\/h2>\n<p>\u70ad\u5316\u30b1\u30a4\u7d20\u88fd\u30ce\u30ba\u30eb\u306f\u3001\u771f\u936e\u3084\u30b9\u30c6\u30f3\u30ec\u30b9\u88fd\u306e\u3088\u3046\u306a\u91d1\u5c5e\u88fd\u30ce\u30ba\u30eb\u3068\u6bd4\u3079\u3066\u3001\u591a\u304f\u306e\u5229\u70b9\u304c\u3042\u308b\u3002\u3053\u308c\u3089\u306e\u5229\u70b9\u306b\u3088\u308a\u30013D\u30d7\u30ea\u30f3\u30c6\u30a3\u30f3\u30b0\u30d5\u30a1\u30f3\u306b\u3082\u30d7\u30ed\u30d5\u30a7\u30c3\u30b7\u30e7\u30ca\u30eb\u306b\u3082\u4eba\u6c17\u304c\u9ad8\u307e\u3063\u3066\u3044\u308b\u3002.<\/p>\n<p>\u3088\u308a\u8010\u4e45\u6027\u304c\u3042\u308b<\/p>\n<p>\u70ad\u5316\u30b1\u30a4\u7d20\u88fd\u30ce\u30ba\u30eb\u306f\u91d1\u5c5e\u88fd\u30ce\u30ba\u30eb\u3088\u308a\u3082\u9577\u6301\u3061\u3057\u307e\u3059\u3002\u975e\u5e38\u306b\u786c\u3044\u306e\u3067\u3001\u70ad\u7d20\u7e4a\u7dad\u8907\u5408\u6750\u6599\u306e\u3088\u3046\u306a\u30d5\u30a3\u30e9\u30e1\u30f3\u30c8\u306e\u7c97\u3055\u306b\u3082\u58ca\u308c\u308b\u3053\u3068\u306a\u304f\u5bfe\u5fdc\u3067\u304d\u307e\u3059\u3002\u305d\u306e\u305f\u3081\u3001\u30e1\u30f3\u30c6\u30ca\u30f3\u30b9\u306b\u304b\u304b\u308b\u8cbb\u7528\u3082\u5c11\u306a\u304f\u3001\u4ea4\u63db\u983b\u5ea6\u3082\u5c11\u306a\u304f\u306a\u308a\u307e\u3059\u3002.<\/p>\n<p>\u71b1\u4f1d\u5c0e\u306b\u512a\u308c\u308b<\/p>\n<p>\u70ad\u5316\u30b1\u30a4\u7d20\u306f\u71b1\u4f1d\u5c0e\u7387\u304c\u9ad8\u304f\u3001\u71b1\u304c\u79fb\u52d5\u3057\u3084\u3059\u3044\u3002\u3053\u308c\u306f\u30d7\u30ea\u30f3\u30c8\u306b\u9069\u3057\u305f\u6e29\u5ea6\u3092\u4fdd\u3064\u305f\u3081\u306b\u91cd\u8981\u3067\u3059\u3002\u3053\u306e\u7279\u6027\u306b\u3088\u308a\u3001\u30d5\u30a3\u30e9\u30e1\u30f3\u30c8\u304c\u5747\u4e00\u306b\u6eb6\u3051\u308b\u305f\u3081\u3001\u30ec\u30a4\u30e4\u30fc\u306e\u5bc6\u7740\u6027\u304c\u5411\u4e0a\u3057\u3001\u9ad8\u54c1\u8cea\u306a\u30d7\u30ea\u30f3\u30c8\u304c\u53ef\u80fd\u306b\u306a\u308a\u307e\u3059\u3002.<\/p>\n<p>\u8a70\u307e\u308a\u306e\u6e1b\u5c11<\/p>\n<p>\u901a\u5e38\u306e\u30ce\u30ba\u30eb\u306e\u554f\u984c\u306e\u3072\u3068\u3064\u306f\u3001\u7279\u306b\u7279\u6b8a\u306a\u30d5\u30a3\u30e9\u30e1\u30f3\u30c8\u3092\u4f7f\u3063\u3066\u30d7\u30ea\u30f3\u30c8\u3059\u308b\u5834\u5408\u306b\u3001\u8a70\u307e\u3063\u3066\u3057\u307e\u3046\u3053\u3068\u3060\u3002\u70ad\u5316\u30b1\u30a4\u7d20\u306e\u6ed1\u3089\u304b\u306a\u8868\u9762\u3068\u4f4e\u3044\u6469\u64e6\u4fc2\u6570\u306f\u3001\u6750\u6599\u304c\u84c4\u7a4d\u3059\u308b\u53ef\u80fd\u6027\u3092\u4f4e\u304f\u3057\u3001\u5370\u5237\u3092\u3088\u308a\u4fe1\u983c\u6027\u306e\u9ad8\u3044\u3082\u306e\u306b\u3059\u308b\u3002.<\/p>\n<p>\u3055\u307e\u3056\u307e\u306a\u30d5\u30a3\u30e9\u30e1\u30f3\u30c8\u306b\u5bfe\u5fdc<\/p>\n<p>\u30b7\u30c3\u30af\u30fb\u30ce\u30ba\u30eb\u306f\u3001PLA\u3001ABS\u3001PETG\u3001\u3055\u3089\u306bPEEK\u3084\u30ca\u30a4\u30ed\u30f3\u8907\u5408\u6750\u306a\u3069\u306e\u9ad8\u5ea6\u306a\u7d20\u6750\u306a\u3069\u3001\u3055\u307e\u3056\u307e\u306a\u7a2e\u985e\u306e\u30d5\u30a3\u30e9\u30e1\u30f3\u30c8\u306b\u5bfe\u5fdc\u3057\u307e\u3059\u3002\u69d8\u3005\u306a\u4f7f\u3044\u65b9\u304c\u3067\u304d\u308b\u305f\u3081\u3001\u30d7\u30ed\u30c8\u30bf\u30a4\u30d4\u30f3\u30b0\u304b\u3089\u5de5\u696d\u751f\u7523\u307e\u3067\u3001\u3042\u3089\u3086\u308b\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002.<\/p>\n<h2>\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306e\u7528\u9014<\/h2>\n<p>\u30b7\u30c3\u30af\u30ce\u30ba\u30eb\u306f\u3001\u305d\u306e\u30e6\u30cb\u30fc\u30af\u306a\u7279\u6027\u304b\u3089\u3001\u3055\u307e\u3056\u307e\u306a\u5206\u91ce\u3067\u3055\u307e\u3056\u307e\u306a\u7528\u9014\u306b\u9069\u3057\u3066\u3044\u308b\u3002.<\/p>\n<p>\u822a\u7a7a\u5b87\u5b99\u3068\u81ea\u52d5\u8eca<\/p>\n<p>\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306f\u3001\u7cbe\u5ea6\u3068\u4fe1\u983c\u6027\u304c\u975e\u5e38\u306b\u91cd\u8981\u8996\u3055\u308c\u308b\u822a\u7a7a\u5b87\u5b99\u7523\u696d\u3084\u81ea\u52d5\u8eca\u7523\u696d\u306b\u304a\u3044\u3066\u3001\u975e\u5e38\u306b\u5f37\u304f\u3001\u8010\u71b1\u6027\u304c\u5fc5\u8981\u306a\u90e8\u54c1\u3092\u88fd\u9020\u3059\u308b\u305f\u3081\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002\u3053\u308c\u3089\u306e\u30ce\u30ba\u30eb\u3092\u4f7f\u7528\u3059\u308b\u3053\u3068\u3067\u3001\u8efd\u91cf\u3067\u3042\u308a\u306a\u304c\u3089\u904e\u9177\u306a\u6761\u4ef6\u4e0b\u3067\u3082\u5341\u5206\u306a\u5f37\u5ea6\u3092\u6301\u3064\u90e8\u54c1\u3092\u5370\u5237\u3059\u308b\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002.<\/p>\n<p>\u533b\u7642\u5668\u5177<\/p>\n<p>\u70ad\u5316\u30b1\u30a4\u7d20\u88fd\u30ce\u30ba\u30eb\u306f\u3001\u8907\u96d1\u306a\u8a2d\u8a08\u3092\u9ad8\u3044\u7cbe\u5ea6\u3067\u884c\u3046\u3053\u3068\u304c\u3067\u304d\u308b\u305f\u3081\u3001\u533b\u7642\u5206\u91ce\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002\u3053\u308c\u3089\u306e\u30ce\u30ba\u30eb\u306f\u3001\u7cbe\u5ea6\u304c\u975e\u5e38\u306b\u91cd\u8981\u306a\u533b\u7642\u6a5f\u5668\u3001\u4eba\u5de5\u88c5\u5177\u3001\u30a4\u30f3\u30d7\u30e9\u30f3\u30c8\u306e\u88fd\u9020\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002.<\/p>\n<p>\u5de5\u5834\u3067\u306e\u3082\u306e\u3065\u304f\u308a<\/p>\n<p>\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u3092\u4f7f\u7528\u3059\u308b\u5de5\u696d\u751f\u7523\u5de5\u7a0b\u306f\u307e\u3059\u307e\u3059\u5897\u3048\u3066\u304a\u308a\u3001\u7279\u306b\u5f37\u5ea6\u304c\u5fc5\u8981\u3067\u9577\u6301\u3061\u3059\u308b\u90e8\u54c1\u3092\u88fd\u9020\u3059\u308b\u969b\u306b\u4f7f\u7528\u3055\u308c\u3066\u3044\u307e\u3059\u3002\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306f\u3001\u7c97\u3044\u6750\u6599\u306b\u3082\u5bfe\u5fdc\u3067\u304d\u308b\u305f\u3081\u3001\u6a5f\u68b0\u3084\u5de5\u5177\u306b\u4f7f\u7528\u3059\u308b\u306e\u306b\u6700\u9069\u3067\u3059\u3002.<\/p>\n<p>\u30c7\u30b6\u30a4\u30f3\u3068\u30a2\u30fc\u30c8<\/p>\n<p>\u30a2\u30fc\u30c6\u30a3\u30b9\u30c8\u3084\u30c7\u30b6\u30a4\u30ca\u30fc\u3082\u3001\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u3092\u4f7f\u3063\u3066\u975e\u5e38\u306b\u7d30\u304b\u304f\u8907\u96d1\u306a\u4f5c\u54c1\u3092\u4f5c\u3063\u3066\u3044\u308b\u3002\u3053\u306e\u30ce\u30ba\u30eb\u3092\u4f7f\u3048\u3070\u3001\u666e\u901a\u306e\u30ce\u30ba\u30eb\u3067\u306f\u96e3\u3057\u304b\u3063\u305f\u8907\u96d1\u306a\u5f62\u3082\u4f5c\u308c\u308b\u3002.<\/p>\n<h2>\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306e\u624b\u5165\u308c\u3068\u30e1\u30f3\u30c6\u30ca\u30f3\u30b9\u65b9\u6cd5<\/h2>\n<p>\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306e\u6027\u80fd\u3092\u6700\u5927\u9650\u306b\u5f15\u304d\u51fa\u3057\u3001\u3067\u304d\u308b\u3060\u3051\u9577\u6301\u3061\u3055\u305b\u308b\u305f\u3081\u306b\u306f\u3001\u9069\u5207\u306a\u30b1\u30a2\u304c\u5fc5\u8981\u3067\u3059\u3002\u304a\u624b\u5165\u308c\u306e\u65b9\u6cd5\u3092\u3044\u304f\u3064\u304b\u3054\u7d39\u4ecb\u3057\u307e\u3059\uff1a<\/p>\n<p>\u3053\u307e\u3081\u306b\u6383\u9664\u3059\u308b\u30d5\u30a3\u30e9\u30e1\u30f3\u30c8\u306e\u6b8b\u6e23\u304c\u6e9c\u307e\u3089\u306a\u3044\u3088\u3046\u306b\u3001\u30ce\u30ba\u30eb\u306f\u5b9a\u671f\u7684\u306b\u6e05\u6383\u3057\u3066\u304f\u3060\u3055\u3044\u3002\u30b9\u30e0\u30fc\u30ba\u306a\u52d5\u4f5c\u3092\u4fdd\u3064\u305f\u3081\u306b\u3001\u67d4\u3089\u304b\u3044\u30d6\u30e9\u30b7\u3084\u5c02\u7528\u306e\u30af\u30ea\u30fc\u30cb\u30f3\u30b0\u30d5\u30a3\u30e9\u30e1\u30f3\u30c8\u3092\u4f7f\u7528\u3057\u3066\u304f\u3060\u3055\u3044\u3002.<br \/>\n\u6e29\u5ea6\u3092\u7ba1\u7406\u3059\u308b\uff1a\u30d7\u30ea\u30f3\u30c8\u306e\u6e29\u5ea6\u304c\u4f7f\u7528\u3059\u308b\u30d5\u30a3\u30e9\u30e1\u30f3\u30c8\u306b\u5408\u3063\u3066\u3044\u308b\u3053\u3068\u3092\u78ba\u8a8d\u3057\u3066\u304f\u3060\u3055\u3044\u3002\u30ce\u30ba\u30eb\u304c\u71b1\u3059\u304e\u308b\u3068\u3001\u6750\u6599\u304c\u58ca\u308c\u3066\u3057\u307e\u3046\u3053\u3068\u304c\u3042\u308a\u307e\u3059\u3002.<br \/>\n\u7814\u78e8\u6750\u306f\u4f7f\u308f\u306a\u3044\u3067\u304f\u3060\u3055\u3044\uff1a\u70ad\u5316\u30b1\u30a4\u7d20\u306e\u30ce\u30ba\u30eb\u306f\u4e08\u592b\u3067\u3059\u304c\u3001\u3042\u307e\u308a\u306b\u7814\u78e8\u6027\u306e\u9ad8\u3044\u6750\u6599\u306f\u4f7f\u7528\u3057\u306a\u3044\u3067\u304f\u3060\u3055\u3044\u3002.<\/p>\n<h2>\u7d50\u8ad6\u3068\u3057\u3066<\/h2>\n<p>\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306f\u3001\u8010\u4e45\u6027\u306b\u512a\u308c\u3001\u9ad8\u6e29\u3067\u3082\u5b89\u5b9a\u3057\u3001\u3055\u307e\u3056\u307e\u306a\u7528\u9014\u306b\u4f7f\u7528\u3067\u304d\u308b\u305f\u3081\u30013D\u30d7\u30ea\u30f3\u30c6\u30a3\u30f3\u30b0\u6280\u8853\u306b\u304a\u3051\u308b\u5927\u304d\u306a\u524d\u9032\u3067\u3059\u3002\u305d\u306e\u30e6\u30cb\u30fc\u30af\u306a\u7279\u6027\u304b\u3089\u3001\u822a\u7a7a\u5b87\u5b99\u304b\u3089\u533b\u7642\u6a5f\u5668\u307e\u3067\u5e45\u5e83\u3044\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002\u9ad8\u6027\u80fd\u5370\u5237\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u3078\u306e\u30cb\u30fc\u30ba\u304c\u9ad8\u307e\u308b\u306b\u3064\u308c\u3001\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306f\u696d\u754c\u6a19\u6e96\u306b\u306a\u308b\u53ef\u80fd\u6027\u304c\u9ad8\u3044\u3002\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306f\u3001\u30e6\u30fc\u30b6\u30fc\u306b\u4fe1\u983c\u6027\u304c\u9ad8\u304f\u52b9\u7387\u7684\u306a\u5370\u5237\u4f53\u9a13\u3092\u3082\u305f\u3089\u3059\u3060\u308d\u3046\u3002.<\/p>\n<p>\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306e\u5229\u70b9\u3068\u7528\u9014\u306b\u3064\u3044\u3066\u77e5\u3063\u3066\u3044\u308b\u4eba\u306f\u30013D\u30d7\u30ea\u30f3\u30c8\u306e\u30cb\u30fc\u30ba\u306b\u3064\u3044\u3066\u8ce2\u3044\u9078\u629e\u3092\u3059\u308b\u3053\u3068\u304c\u3067\u304d\u308b\u3002\u305d\u3046\u3059\u308b\u3053\u3068\u3067\u3001\u3088\u308a\u826f\u3044\u7d50\u679c\u304c\u5f97\u3089\u308c\u3001\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306e\u6e80\u8db3\u5ea6\u3082\u9ad8\u307e\u308b\u3002.<\/p>","protected":false},"excerpt":{"rendered":"<p>3D\u30d7\u30ea\u30f3\u30c6\u30a3\u30f3\u30b0\u306b\u304a\u3044\u3066\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u304c\u512a\u308c\u3066\u3044\u308b\u7406\u7531 \u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306f\u3001\u4ed6\u306e\u3069\u306e\u30ce\u30ba\u30eb\u306b\u3082\u5339\u6575\u3057\u306a\u3044\u6027\u80fd\u3068\u8010\u4e45\u6027\u3092\u63d0\u4f9b\u3059\u308b\u3053\u3068\u3067\u30013D\u30d7\u30ea\u30f3\u30c6\u30a3\u30f3\u30b0\u306e\u5e38\u8b58\u3092\u4e00\u5909\u3055\u305b\u307e\u3057\u305f\u3002\u3053\u308c\u3089\u306e\u30ce\u30ba\u30eb\u306f\u3001\u975e\u5e38\u306b\u786c\u304f\u3001\u9ad8\u6e29\u4e0b\u3067\u3082\u5b89\u5b9a\u3057\u3066\u3044\u308b\u3053\u3068\u3067\u77e5\u3089\u308c\u308b\u7d20\u6750\u3067\u4f5c\u3089\u308c\u3066\u3044\u308b\u305f\u3081\u3001\u591a\u304f\u306e\u30d7\u30ea\u30f3\u30c6\u30a3\u30f3\u30b0\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002 \u672c\u8a18\u4e8b\u3067\u306f\u3001\u70ad\u5316\u30b1\u30a4\u7d20\u30ce\u30ba\u30eb\u306e\u7279\u5fb4\u3001\u5f93\u6765\u306e\u7d20\u6750\u306b\u6bd4\u3079\u3066\u512a\u308c\u3066\u3044\u308b\u70b9\u3001\u305d\u3057\u3066\u3055\u307e\u3056\u307e\u306a\u7523\u696d\u3067\u306e\u6d3b\u7528\u65b9\u6cd5\u306b\u3064\u3044\u3066\u89e3\u8aac\u3057\u307e\u3059\u3002\u70ad\u5316\u30b1\u30a4\u7d20\u306b\u3064\u3044\u3066 \u70ad\u5316\u30b1\u30a4\u7d20\uff08SiC\uff09\u306f\u3001\u30b1\u30a4\u7d20\u3068\u70ad\u7d20\u304c\u7d50\u5408\u3057\u305f\u5316\u5408\u7269\u3067\u3042\u308a\u3001\u975e\u5e38\u306b\u8208\u5473\u6df1\u3044\u7269\u7406\u7684\u30fb\u5316\u5b66\u7684\u7279\u6027\u3092\u6709\u3057\u3066\u3044\u307e\u3059\u2026\u2026\u3002&nbsp;<\/p>","protected":false},"author":1,"featured_media":0,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"neve_meta_sidebar":"","neve_meta_container":"","neve_meta_enable_content_width":"","neve_meta_content_width":0,"neve_meta_title_alignment":"","neve_meta_author_avatar":"","neve_post_elements_order":"","neve_meta_disable_header":"","neve_meta_disable_footer":"","neve_meta_disable_title":"","ngg_post_thumbnail":0,"footnotes":""},"categories":[30],"tags":[],"class_list":["post-676","post","type-post","status-publish","format-standard","hentry","category-sic-knowledge"],"aioseo_notices":[],"_links":{"self":[{"href":"https:\/\/siliconcarbide.net\/ja\/wp-json\/wp\/v2\/posts\/676","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/siliconcarbide.net\/ja\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/siliconcarbide.net\/ja\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/siliconcarbide.net\/ja\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/siliconcarbide.net\/ja\/wp-json\/wp\/v2\/comments?post=676"}],"version-history":[{"count":1,"href":"https:\/\/siliconcarbide.net\/ja\/wp-json\/wp\/v2\/posts\/676\/revisions"}],"predecessor-version":[{"id":677,"href":"https:\/\/siliconcarbide.net\/ja\/wp-json\/wp\/v2\/posts\/676\/revisions\/677"}],"wp:attachment":[{"href":"https:\/\/siliconcarbide.net\/ja\/wp-json\/wp\/v2\/media?parent=676"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/siliconcarbide.net\/ja\/wp-json\/wp\/v2\/categories?post=676"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/siliconcarbide.net\/ja\/wp-json\/wp\/v2\/tags?post=676"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}