Silicon carbide powder is also known as emery, products are hexagonal crystals, specific gravity 3.20-3.25, Mohs hardness 9.2, microhardness 2840-3320kg/mm2. silicon carbide has the properties of stable chemical properties, high thermal conductivity, small coefficient of thermal expansion, and good abrasion resistance.Silicon carbide powder has many major application areas,such as functional ceramics,structural ceramics, advanced refractories, abrasives and metallurgical and so on. (1) Abrasive silicon carbide powder can be used as grinding media or grinding auxiliary material for grinding...