nitride bonded silicon carbide

Nitride bonded silicon carbide is a new type of advanced refractory. Its main products include silicon nitride bonded silicon carbide radiation tubes, bricks, nitride bonded silicon carbide shelves and so on

Performance and use

1.nitride bonded sic, with a hard texture and a Mohs hardness of about 9, are hardness materials in non-metallic materials, second only to diamond.

2. The strength and hardness of nitride bonded silicon carbide kiln shelves are high at room temperature. At 1200-1400 C, the strength and hardness of nitride bonded silicon carbide are almost the same as those at room temperature for the same time. With the use of different atmospheres, the maximum safe use temperature can reach 1650-1750 C.

3. The thermal expansion coefficient of silicon nitride bonded silicon carbide is small. Compared with silicon carbide and other products, the thermal conductivity is higher. It is not easy to produce thermal stress. nitride bonded sic has good thermal shock stability and long service life. High temperature creep resistance, corrosion resistance, extreme cold and heat resistance, oxidation resistance, easy to make products with high dimensional accuracy and meet the requirements.

4. silicon nitride bonded silicon carbide are widely used in iron and steel, non-ferrous metals, chemical building materials and other industries, energy saving, environmental protection, cost reduction.