Effect of additives on sintered silicon carbide

Pressureless sintered silicon carbide is considered to be the most promising sintered silicon carbide, and complex shapes and large sizes of silicon carbide ceramics can be prepared by the pressureless sintering process. Depending on the… 

Structure and Crystallization of SiC

  • by

SiC is a covalently bonded compound with strong bonding between Si-C, has a diamond structure, and has 75 crystalline forms. The basic structural unit of its lattice is the covalently bonded [SiC4] and [CSi4] tetrahedral… 

sintered silicon carbide

technology of sintered silicon carbide

  • by

silicon carbide ceramic are more and more widely used because of their excellent high temperature strength, wear resistance, corrosion resistance and thermal shock resistance. SiC ceramics play an increasingly important role in the field of… 

sisic ceramic

Reaction Bonded Silicon Carbide

  • by

Manufacturers are looking for more energy-efficient engines and want to replace critical metals. These motives initiated the development of different ceramic materials and processes. Reaction bonded silicon carbide is a result of these investigations.Reaction bonded… 

green silicon carbide powder

silicon carbide powder

  • by

Silicon carbide powder is also known as emery, products are hexagonal crystals, specific gravity 3.20-3.25, Mohs hardness 9.2, microhardness 2840-3320kg/mm2. silicon carbide has the properties of stable chemical properties, high thermal conductivity, small coefficient of… 

recrystallized silicon carbide

recrystallized silicon carbide

  • by

Coarse raw materials and fine SiC powders are formed, under the protection of high temperature and certain pressure,they are recrystallized by vacuum sintering,by evaporation of fine SiC powders and coagulation in coarse SiC particles.,then we… 

nitride bonded silicon carbide

  • by

Nitride bonded silicon carbide is a new type of advanced refractory. Its main products include silicon nitride bonded silicon carbide radiation tubes, bricks, nitride bonded silicon carbide shelves and so on Performance and use 1.nitride… 

flue gas desulfurization nozzle

silicon carbide nozzle for flue gas desulfurization

  • by

Desulfurization nozzle for power plant desulfurization, removal of sulfur dioxide and some polluting gases in the flue gas of power plants. The vacuum reaction bonded silicon carbide desulfurization nozzle is the key component of the power… 

silicon carbide bulletproof ceramic

silicon carbide bulletproof ceramic

  • by

this kind of silicon carbide bricks is made of super fine sintered silicon carbide powder with excellent thermal conductivity, high temperature resistant, high temperature resistant to oxidation, corrosion resistance, acid and alkali, solvent and other… 